Available thickness: 12micron, 15micron, 19micron and 25 micron.


JT03 Cross-Linked Shrink Film
TEST ITEM UNIT ASTM TEST TYPICAL VALUES
THICKNESS     12um 15um 19um 25um 30um
TENSILE
Tensile Strength (MD) N/mm2 D882 131 136 136 136 136
Tensile Strength (TD) 126 126 126 131 131
Elongation (MD) % 126 131 131 141 141
Elongation (TD) 121 126 121 131 136
TEAR
MD g D1922 10.1 14.6 17.6 25.6 33.6
TD 9.1 13.6 16.6 25.1 30.1
SEAL STRENGTH
MD/Hot Wire Seal N/mm F88 1.43 1.39 1.55 1.85 2.25
TD/Hot Wire Seal 1.28 1.53 1.75 1.85 2.20
COF(film to Film)
Dynamic   D1894 0.33 0.30 0.32 0.35 0.35
Static   0.35 0.31 0.33 0.37 0.35
OPTICS
Haze   D1003 2.4 2.7 3.6 3.9 4.3
Clarity   D1746 98.6 98.9 98.1 97.6 94.1
Gloss @ 45Deg   D2457 88.6 88.1 87.6 86.1 86.1
BARRIER
Oxygen Transmission Rate cc/m2/day D3985 10300 9500 6200 5400 4200
Water Vapor Transmission Rate gm/m2/day F1249 34.6 29.6 21.6 15.6 12
SHRINKAGE PROPERTIES MD TD
Free Shrinkage 100℃ % D2732 17 27
110℃ 35 44
120℃ 63 67
130℃ 82 80
Shrink Tension 100℃ Mpa D2838 2.20 2.65
110℃ 2.80 3.95
120℃ 3.00 4.35
130℃ 2.90 4.1
Note: This infor mation represents our best judgment on the work done,but the company assumes no liability whatsoever in connection with the use of infomation or findings contained herein.
DownloadInquiry

Copyright © 2010 ZHEJIANG JUE TENG PACKAGING. All rights reserved. | ZHE ICP BEI 10210939-1

W3C XHTML | W3C CSS | GO TOP